產(chǎn)品詳情
AWS型號 |
產(chǎn)品牌號 |
焊絲化學(xué)成份 |
特性簡單介紹 |
||||||
|
|
C |
Mn |
Si |
S |
P |
|
|
|
ER70S-3 |
NERTALIC 70S |
0.08 |
1.15 |
0.6 |
0.015 |
0.015 |
|
|
|
ER70S-6 |
NERTALIC 70A |
0.08 |
1.4 |
0.8 |
0.015 |
0.015 |
|
|
|
ER80SG |
CARBOFIL Cr Mo 1 |
0.08 |
1.4 |
0.8 |
|
Mo:0.6 Cr:1.1 |
焊接σs≥420Mpa高強鋼 |
||
ER100S-G |
NERTALIC 88 |
0.05 |
1.9 |
0.45 |
0.010 |
0.010 |
Ni:2.0 Mo:0.55 |
焊接σs≥650Mpa高強鋼,用于ELDOX 700鋼,WEDOX900低強匹配焊 |
|
ER110S-G |
CARBOFIL Ni Mo Cr |
≤0.01 |
1.6 |
0.6 |
|
Ni:1.4,Mo:0.25,Cr:0.3 |
焊接σs≥690Mpa高強鋼,用于WELDOX 700鋼,WEDOX900低強匹配焊 |
||
ER90S-G |
CARBOFIL Ni Mo 1 |
≤0.10 |
1.8 |
0.6 |
|
|
Ni:1.0 Mo:0.4 Ti:0.15 |
焊接σs≥620Mpa高強鋼 |
|
ER120S-G |
ED-FK 1000 |
0.10 |
1.80 |
0.80 |
|
Mo:0.50,Ni:2.20 |
焊接σs≥620Mpa高強鋼,用于WELDOX900,960鋼 |
Category |
Trade- |
Equivalent to China Standard |
Characteristics & application |
Equivalent to AWS |
Hard-surfacing 硬 面
堆
焊
|
D 667 |
EDZCr-B-15 |
HRc≥48. Resistance to wear, gas corrosion and oxidation. Hardfacing of blast furnace hopper and cracker part. |
|
D 802 |
EDCoCr-A-03 |
HRc38-47. Resistance to heat, wear and corrosion. Hardfacing of high temperature part such as the edge of thermo-cutter. |
ECoCr-A |
|
D 812 |
EDCoCr-B-03 |
HRc45-50. Resistance to heat, wear and corrosion. Hardfacing of high temperature part such as internal-combustion engine valve. |
ECoCr-B |
|
D 822 |
|
HRc≥53. Resistance to Wear and heat, bad shock resistance. Hardfacing of rotating blade wheel of boiler. |
|
|
D 832 |
EDCoCr-C-03 |
HRc≥50. Wear and heat resistance. Hardfacing of high temperature part such as hot-rolling guided way. |
ECoCr-C |
|
D 842 |
EDCoCr-D-03 |
HRc28-38. Corrosion and thermo-fatigue resistance, work harding. Hardfacing of hot forging die. |
|
|
Cast iron
鑄
鐵 |
Z 308 |
EZNi |
Pure nickel, excellent general properties. Used to weld thin cast iron part and repair welding machined surface, such as guided way of machine tool. |
ENi-Cl |
Z 408 |
EZNiFe |
Iron nickel, high strength and excellent ductility. Repair welding of important gray cast iron and nodular cast iron, such as cylinder cap. |
ENiFe-Cl |
|
Z 508 |
EZNiCu-1 |
Copper nickel, good machinability and bad crack resistance. Repair welding of sand hole and gray cast iron machined surface subject to no load. |
ENiCu-B |
|
Copper alloys
銅
合
金 |
Cu 107 |
ECu |
Red copper, atmosphere and sea water corrosion and excellent electric conductivity. Welding of red copper such as electrical copper row. |
ECu |
Cu 207 |
ECuSi |
Silicon bronze, corrosion resistance and high strength. Welding of copper, silicon bronze and brass. |
ECuSi |
|
Cu 227 |
ECuSnB |
Tin phosphor bronze, corrosion resistance and high strength. Welding of copper, silicon bronze and brass. |
ECuSn-C |
|
Cu 237 |
ECuAl |
Aluminum bronze, wear and corrosion and high strength. Welding or surfacing of copper alloys. |
ECuAl-A2 |
|
Aluminum alloys
鋁 合 金 |
Al 109 |
TAl |
Pure aluminum, excellent corrosion resistance and middle strength. Welding of pure aluminum. |
E1100 |
Al 209 |
TAlSi |
Silicon aluminum, good crack resistance and wide range of usage. Welding of aluminum alloys other than aluminum magnesium alloys. |
E4043 |
|
Al 309 |
TAMn |
Manganese aluminum, corrosion resistance and high strength. Welding of aluminum alloys. |
E3003 |
|
Nickel alloys 鎳合金 |
Ni 102 |
ENi-1 |
Pure nickel. Welding and surfacing of nickel and nickel to steel. |
ENi-1 |
Ni 207 |
ENiCu-7 |
Copper nickel. Welding and surfacing of copper nickel and copper nickel to steel. |
ENiCu-7 |
Category 類別 |
Trade 牌號 |
Chemical comb 主要成份(%) |
Characteristics & application 特性和用途 |
Equivalent to AWS 相當(dāng)AWS |
Hardfacing
硬
面
堆
焊 |
S 101 |
C3 Cr28 Ni4 |
HRc48-54. Resistance to wear, gas corrosion and oxidation. Hardfacing of bucket tooth and case pump. |
|
S 111 |
C1 Cr29 W5 |
HRc38-47. Resistance to wear and corrosion at high-temperature. Hardfacing of high temperature and pressure valve. |
ECoCr-A |
|
S 112 |
C1.5 Cr29 W8 |
HRc45-50. Resistance to wear and corrosion at high-temperature. Hardfacing of valve and hot-rolling pass. |
ECoCr-B |
|
S 113 |
C2.5 Cr30 W17 |
HRc≥55. Wear and heat resistance at high temperature, bad shock resistance. Hardfacing of screw charging carriage. |
|
|
S 114 |
C2.5 Cr30 W12 |
HRc≥53. Wear and heat resistance at high temperature, bad shock resistance. Hardfacing of three-cone bit. |
ECoCr-C |
|
Copper alloys
銅
合
金 |
S 201 |
Sn1 Si0.3Mn0.3 |
Good mechanical properties and crack resistance. Gas welding and argon arc welding of red copper. |
ERCu |
S 211 |
Si3 Mn1 |
Good mechanical properties. Argon arc welding of copper alloys and MIG brazing of steel. |
ERCuSi-Al |
|
S 212 |
Sn5 Cu Rem. |
Wear resistance. Argon arc welding of copper alloys and surfacing of steel. |
ERCuSn-A |
|
S 213 |
Sn8 Cu Rem. |
Wear resistance. Argon arc welding of copper alloys and surfacing of steel. |
ERCuSn-C |
|
S 214 |
Al7.5 Cu Rem. |
Wear and corrosion resistance. Argon arc welding of copper alloys and surfacing of steel. |
ERCuAl-A1 |
|
S 215 |
Al9 Cu Rem. |
Wear and corrosion resistance. Argon arc welding of copper alloys and surfacing of steel. |
ERCuAl-A2 |
|
S 221 |
Cu60 Sn1 Si0.3 |
Melting point is about 890℃. Gas welding and carbon arc welding of brass, also braze welding of copper, steel and cast iron. |
|
|
S 221F |
Cu60 Sn1 Si 0.3 |
S221 welding rod coated with flux. |
|
|
S 222 |
Cu58Sn0.9Si0.1 |
Melting point is about 880℃. Gas welding and carbon arc welding of brass, also braze welding of copper, steel and cast iron. |
RBCuZn-C |